N'oge a na-ekpe ikpe ebu, a na-emekarị ntụpọ ịkpụzi na-enweghị amụma n'ezie, ya mere ezigbo onye injinia na-anwale ịkpụzi kwesịrị inwe ahụmịhe bara ụba iji kpee ihe kpatara ya ngwa ngwa o kwere mee, n'ihi na ọnụ ahịa na-abawanye na oge ejiri na igwe injection.
N'ebe a, ndị otu anyị chịkọbara ụfọdụ ahụmahụ, ọ bụrụ na nkesa a nwere ike igosi ntakịrị ntụle iji rite uru na ngwọta nsogbu gị yiri ya, anyị ga-enwe obi ụtọ.
N'ebe a, anyị na-ekwu maka akara atọ: "Akara ọkụ", "Akara mmiri" na "Akara ikuku".
Atụmatụ:
·Na-apụta kwa oge
·Na-apụta na mpaghara obe dị warara ma ọ bụ ọnọdụ ọnyà ikuku
·Okpomọkụ na-agbaze fọrọ nke nta ka ọ bụrụ oke elu nke okpomọkụ injection
·Nrụrụ ahụ nwere mmetụta ụfọdụ site n'ibelata ọsọ nke ịghasa pịa
·Oge Plasticization dị ogologo, ma ọ bụ nọrọ n'ihu nke screw pịa ogologo oge
·A ga-eji ihe plastik emegharịrị emegharị gabiga ókè ma ọ bụ agbazewo ihe ọtụtụ ugboro tupu mgbe ahụ
·Na-apụta na ebu na usoro ịgba ọsọ na-ekpo ọkụ
·Akpụkpọ nwere nozzle mechiri emechi (Mechie Nozzle)
Atụmatụ:
3. Akara ikuku
N'ozuzu, ikuku akara' shapes bụ ike siri ike, na ọlaọcha ma ọ bụ na-acha ọcha na agba, na-apụtakarị na okirikiri / curved elu, ọgịrịga / mgbidi ọkpụrụkpụ mgbanwe ebe ma ọ bụ na nso nke nozzle, ọnụ ụzọ ámá na-emekarị na-egosi mkpa oyi akwa nke ikuku akara; Akara ikuku na-apụtakwa na ihe osise, dịka ọmụmaatụ: ihe osise ederede ma ọ bụ mpaghara ịda mbà n'obi.
Ewezuga ụdị dị n'elu, anyị nwekwara "Akara Glass-Fiber" na "Akara Agba" n'akụkụ akụkụ ahụ. ya mere n'ọdịnihu, a ga-ekekọrịta ahụmịhe nrụzi ọzọ na ndị enyi m hụrụ n'anya na linkin, ọ bụrụ na ị nwere echiche dị iche iche gbasara post m, biko jiri obiọma mee ka m mara ihe gị, dị ka anyị si mara, linkedin bụ mgbe ọ bụla ikpo okwu dị mma maka anyị ịkọrọ, mụta na imeziwanye!
Oge nzipu: Ọktoba 26-2020